Marine environments postulant welding materiae, quod potest sustinere dura conditionibus, inter saltwater corrosio, altus humiditas, et constant accentus. Inter available optiones, (V) CLIV Aluminium Welding Wire Exserit ex ut a summo choice pro navicula builders, shipyards et marine instaurare doctorum.
I. Superior corrosio resistentia
Saltwater valde mysterium et vexillum ferro vel humilis gradus aluminium fila deficere cito. (V) CLIV Aluminium Welding filum continet magnesium (2.5-3.5%), quod significantly enhances resistentiam ad:
Saltwater corrosio
Pitting et Crevice Corrosion
Accentus corrosio fregisset
Comparatio data:
(V) CLIV (IV) XLIII Aluminium Wire: (V) CLIV habet melius saltwater corrosio resistentia ex superiore magnesium contentus.
(V) CLIV vs. (V) CCCLVI Aluminium Wire: utrumque resistere corrosio bene, sed (V) CLIV praestat melius in altus-humorem marine conditionibus.
II. Altum vires et diuturnitatem
Marine structuris, ut naviculam Hulls et Navks, requirere fortis welds quod potest pati constans motus et impulsum. (V) CLIV Welding filum providet:
Tensile vires: usque ad CCXL MPa
Optimum lassitudine resistentia fluctus-adductus accentus
Ductility bonum, reducendo crack metus in Welded articulis
III. Specimen ad marine-gradu aluminium Alloys
(V) CLIV filer filum est communiter ad Weld:
(V) LXXXIII & (V) LXXXVI Aluminium (Clementine_Vulgate in navi Hulls)
(V) LII Aluminium (in marine caeruleo et blasphemiam)
Et compatibility ensures fortis, crack-liberum welds in discrimine marine components.
Res | 5154 | 5356 | 4043 |
---|---|---|---|
Corrosio resistentia | Praeclarus | Bonum | Moderor |
Fortitudo | Altum | High | Medium |
Optimum | Saltwater applications | General Marine Usus | Freshwater / Minimum-accentus Welds |
Magnesium contentus | 2.5-3.5% | 4.5-5.5% | 0% |
Tensile viribus | Ad CCXL MPa | Ad CCXC MPa | Ad CLXXX MPa |
Elige (V) CLIV ad maximum corrosio resistentia in saltwater.
(V) CCCLVI est bonum alternative ad General Marine Welding sed non novissimis quam diu in extrema condiciones.
Vitare (IV) XLIII ad discrimine marine structurae, caret satis viribus et corrosio resistentia.
Ut fortissimum, longissimum-perpetua marine welds:
Uti MIG Welder cum pulsed RAMULUS serie ad lautus, spatter libero welds.
Pre-emundare basis metallum ad removendum oxidatio et contaminantium.
Ponere propriis protegit Gas (Argon aut Argon / Helium Mix) ut Porosity.
Store filum in sicco loco, humorem potest ducere ad Hydrogenii cracking.3333